We offer OEM/ODM service and prioritize delivering high-quality products in a timely manner. Join us as our partner today!
This product is a solvent-free, low viscosity, room temperature curing two-component polyurethane foam. Very low water absorption, heat and cold shock resistance, excellent weather resistance, and can be cured in low temperature environment.
This product can be used for dust-proof, water-proof, fire-proof, moisture-proof and anti-condensation sealing at the bottom of various electrical cabinets and communication cabinets, as well as smoke, dust and insect prevention sealing of floor or wall components.
Pre curing characteristics |
||||
Component A (main agent) |
Component B (curing agent) |
|||
Typical value |
Range |
Typical value |
Range |
|
Appearance |
Black liquid |
|
Brown liquid |
|
Chemical composition of base material |
Polyhydric alcohols |
|
Isocyanate |
|
Density (g/cm3, 25℃) |
1.22 |
1.22 ± 0.1 |
1.22 |
1.22 ± 0.05 |
Viscosity (mPa.s, 25℃) |
1000 |
800 ±500 |
220 |
200 ± 100 |
Mixed characteristic |
||||
Typical value |
Range |
|||
Appearance |
Dark gray |
|
||
Mixed weight ratio |
A:B =100:100 |
|
||
Mixed weight ratio |
3 |
2~10 | ||
Drawing time (Sec) |
10 |
10~20 | ||
Non-stick time (Sec) |
30 |
30~60 | ||
Percentage of closed pores (%) |
≥88 |
90 | ||
Oxygen index (%) |
≥25 |
27 | ||
Water absorption (%) |
≤6 |
5 | ||
Low temperature dimensional stability (%) |
≤1 |
1 | ||
High temperature dimensional stability (%) |
≤1.2 |
1.2 |
5.When testing the flame retardant performance, the rubber strip should be completely cured. Incomplete curing of the rubber strip will affect the flame retardant performance test results.